The compressive strengths from the concrete cylinders are the main focus of this report although air and proctor tests were also conducted.

The tests conducted in the LAOP conform with the standards approved by the American Society of Testing Materials (ASTM) which are briefly described in Appendix A of the report.

This report will focus on five admixtures tested on four different Lafarge cements. One of the admixtures was targeted for possible future commercial use. A brief profile of all of the admixtures and the cement used is given within the report. It was concluded that the admixture called 325-N would yield the highest strength over a 28 day period. It was only better by less than 4% in comparison to the compressive strengths of the other admixtures. Further details on each of the individual trial mixes can be found in Appendix B.

It is recommended that when conducting a program similar to this one that the initial set times and the 24 hour compressive strengths be eliminated as their result reflect to no certain extent how the concrete will stand up over a 28 day period.

Although Lafarge uses similar processes to manufacture cements at all of its locations across Ontario, the cement


The batching procedure for each mix in the LAOP went as follows:

While a cement manufacturer might design a cement to work dynamically with various aggregates, it has never been a task for the cement manufacturer to make a cement to work better with an admixture. It is the task of the admixture manufacturer to refine an admixture until it works properly with the cement or at least until the desired effect on the concrete has been accomplished. This comes as no surprise as admixtures were invented to improve upon the cements abilities to create a better concrete.



Some common words found in the essay are:
Abstract Lafarge, Doseml/batch Dosageml/kg, Constant Wookstock, Water Reducers, Materials ASTM, Constant Woodstock, CSA CSA, St Constant, Summary Conclusion, , compressive strengths, water reducer, initial set, standard test method, admixtures tested, st constant, compressive strength, test method, 325 3575, standard test, control mix, 3575 450 4950, 325 3575 450, ideal water reducer, cement mix doseml/batch,

Approximate Word count = 2505
Approximate Pages = 10 (250 words per page double spaced)

join now Save Paper



Saved Paper

Save your papers so you can locate them quickly!

Newest Essays

Testimonials

  • "Thank You So Much!!! You have saved me once again!!!"
    Jack M.
  • "With so many papers to chose from, I was able to get ideas to help me with all of my classes. Thank You!"
    Brian P.
  • "I've used this site for the last 3 years to help me come up with ideas for my papers."
    Sara J.
  • "I use this site every week to help me write my own papers!"
    Rachel W.
  • "I love this site!!!"
    Marie N.